Oxidación húmeda de fenoles con catalizadores Fe-CeO2, K-MnO2/ CeO2/Paligorsquita y Fe/ paligorsquita

The performance of Fe-MnO2/CeO2, K-MnO2/CeO2/ Palygorskite and Fe/ Palygorskite catalysts during the wet oxidative degradation of phenol in a stirred reactor has been evaluated. The experiments were run at 130°C, 20.4 atm., and with an initial phenol and catalyst mass concentration of 0.5 g/L and 5...