This work focused on fracture toughness studies of WC–10 wt% Co hardmetal fabricated through the high pressure/high-temperature technique. A powder mixture of WC–10 wt% Co was sintered at 1500–1900°C under a pressure of 7.7 GPa for 2 and 3 min. Vickers hardness test at two different loads of 15 and...