1“..., characterized, shaped by uniaxial pressing and sinterized in the temperatures of 940ºC, 1000ºC, 1060ºC, 1120ºC...”
Mais informações
doctoralThesis -
2“... pressing and sinterized in the temperatures of 940ºC, 1000ºC, 1060ºC, 1120ºC and 1180ºC, using a fast...”