1por Melo, Marcus Antônio de Freitas, Câmara, Ana Paula Costa, Medeiros, L. C. de, Macedo, D. A. de, Melo, Dulce Maria de Araújo“... after sintering between 850 and 1050°C. The technological properties evaluated were: linear shrinkage...”
Mais informações
article -
2“... in the ceramic matrix. After sintering at temperatures 1080, 1120 and 1160 °C, the samples were tested for water...”
Mais informações
doctoralThesis -
3por Câmara, Ana Paula Costa., Melo, Marcus Antônio de Freitas., Duarte, Márcia Maria Lima., Universidade Federal do Rio Grande do Norte.“..., 10 and 20 % by weight of gravel in the ceramic matrix. After sintering at temperatures 1080, 1120...”
Mais informações
Tese