Bond strength enhancement of metal-ceramic dental restorations by FGM design /

Abstract: Bond strength enhancement of metal-ceramic dental restorations by FGM design Metal ceramic dental restorations are widely used in dental prosthetics due to their good esthetic properties but mainly because of their higher survival rates when compared to other restorative systems. Neverthe...

ver descrição completa

Na minha lista:
Detalhes bibliográficos
Principais autores: Henriques, Bruno Alexandre Pacheco de Castro., Silva, Filipe Samuel Correia Pereira., Soares, Delfim Fernandes., Universidade do Minho.
Formato: Tese
Publicado em:
Assuntos:
Endereço do item:https://app.bczm.ufrn.br/home/#/item/215006
Tags: Adicionar Tag
Sem tags, seja o primeiro a adicionar uma tag!
id oai:localhost:123456789-142380
record_format dspace
institution Acervo SISBI
collection SIGAA
topic Engenharia mecânica -
Tese.
Restaurações metalocerâmicas -
Dentes -
Tese.
Gradiente funcional de propriedades(FGMs) -
Tese.
Durabilidade -
Sucesso -
Tese.
spellingShingle Engenharia mecânica -
Tese.
Restaurações metalocerâmicas -
Dentes -
Tese.
Gradiente funcional de propriedades(FGMs) -
Tese.
Durabilidade -
Sucesso -
Tese.
Henriques, Bruno Alexandre Pacheco de Castro.
Silva, Filipe Samuel Correia Pereira.
Soares, Delfim Fernandes.
Universidade do Minho.
Bond strength enhancement of metal-ceramic dental restorations by FGM design /
description Abstract: Bond strength enhancement of metal-ceramic dental restorations by FGM design Metal ceramic dental restorations are widely used in dental prosthetics due to their good esthetic properties but mainly because of their higher survival rates when compared to other restorative systems. Nevertheless, they still encompass some medium to long term clinical failures, which puts patients back to the dentists' chair, causing uncomfortable interventions and undesired money expenditures. This work is concerned with the development of FGM's (Functionally Graded Material) based solution that enhances metal-ceramic bond strength aiming at increasing of long term survival rates of metal-ceramic dental restorations and with the study of the variables that affect metal-ceramic bond strength. The variables that were subjected to study were the hot pressing, the surface treatment, the type of processing used to produce metal substructures, and the preoxidation heat treatment. The hot pressing technique revealed to have significant (p<0.05) influence on the metal-ceramic bond strength, resulting in composites with significantly (p<0.05) higher bond strength values when compared to those obtained by conventional PorcelainFused-to-Metal technique for high gold dental alloys and for CoCrMo dental alloys. In the same way, the hot pressing technique also produced a significant enhancement on porcelain shear strength relative to the conventional vacuum sintered porcelain. The flawless metal-ceramic interfaces and the absence of pores within ceramics thus produced were regarded for the bond strength and cohesion improvements, respectively. The metal-ceramic adhesion was also assessed for different surface treatments of the metal substructure, namely polished and rough surfaces. Porcelain exhibited higher adhesion to rough metal substrates than to polished ones. The mechanical interlocking and the higher surface area for chemical bonding caused the bond strength improvements seen in rough surfaces. The CoCrMo alloy obtained by casting and hot pressing was assessed in terms of microstructure, corrosion resistance, hardness and metal-ceramic bond strength The casted alloy exhibited a dendritic microstructure whereas the hot pressed alloy exhibited a globular microstructure. The hot pressed alloy revealed higher hardness due to a finer microstructure. The finer microstructure was also regarded for the enhanced corrosion resistance of hot pressed alloys over casted alloy. No significant differences were found in metal-ceramic bond strength between the two types of processing techniques. The preoxidation heat treatment, performed in CoCrMoSi dental alloy, significantly (p<0.05) affected the metal-ceramic bond strength. Non-preoxidized specimens exhibited higher metal-ceramic bond strength than preoxidized/ground ones. The lower bond strength results observed in preoxidized/ground specimens were originated by the presence of oxide remnants on their metal surface after grinding and by the higher oxide thickness formed at the metal-ceramic interface. All preoxidized specimens exhibited adhesive failure type while non-preoxidized presented both adhesive and mixed failure types. Preoxidation heat treatment revealed a detrimental effect on the adhesion of CoCrMoSi-porcelain composites for dental restorations. Several metal/ceramic composites were used as interlayers aiming at the improvement of the bond strength between metal and ceramic, following a FGM approach. Two types of alloys were tested, namely a high-noble alloy and a CoCrMo alloy. Both alloys showed significant (p<0.05) improvements in the metal-ceramic bond strength when using a graded transition provided by the metal/ceramic composite interlayer. The metal particles of the composite interlayer acted as a reinforcing phase that increased the fracture strength of the composite interlayer and improved the strength of the metal-interlayer-ceramic system. The bond strength improvements, relative to conventional PFM technique, proved to be in excess of 140%. The newly developed FGM approach for dental metal-ceramic dental restorations was also evaluated in terms of its performance under thermo-mechanical fatigue conditions. These new functionally graded restorations showed significantly (p<0.05) higher performance under fatigue conditions relative to conventional PFM restorations. The bond strength results showed that the presence of a composite interlayer at the interface significantly (p<0.05) improves the adhesion between the two materials under fatigue conditions, relative to those found in conventional PFM technique. The reduction of the properties mismatch at the metal-ceramic interface of the functionally graded restorations was considered to be the main cause for the bond strength improvements after fatigue tests. Improvements in the range of 210% were observed for the most severe testing conditions. In the end of this work, a preliminary test comprising the manufacture of a graded metal-ceramic dental restorations in real crows were conducted. The restorations were fabricated using the hot pressing technology currently available in dental prosthetic laboratories. This process produced crowns with a good quality of the bond between metal and ceramic. Moreover, no geometric restraints or others were observed to the restorations' proceedings.#$&Resumo: Os restauros dentários metalocerâmicos são muito usados em prótese dentária devido às suas boas propriedades estéticas, mas sobretudo devido às suas elevadas taxas de sucesso clínico comparativamente com outros sistemas de restauro. Contudo, apesar de menos frequentes, também eles apresentam falhas clínicas a médio e longo prazo que fazem com que o paciente regresse à cadeira do dentista, causando intervenções desconfortáveis e gastos desnecessários de dinheiro. Assim, esta tese prende-se com o desenvolvimento de novos sistemas metal-cerâmico para restauro dentário recorrendo ao conceito dos materiais com gradiente funcional de propriedades(FGMs) tendo em vista o aumento da durabilidade e da taxa de sucesso clínico deste tipo de restauro. Esta tese também se debruçou sobre o estudo de variáveis que afetam o resitência da ligação metal-cerâmico. As variáveis alvo de estudo foram: a prensagem a quente, o tratamento superficial, o topo de processamento das substruturas metálicas e o tratamento de pré-oxidação. A técnica de prensagem a quente revelou uma influência significativa(p<0.05) na resitência mecânica da ligação metal-cerâmico, dando origem a compósitos com resitâncias de ligação significativamente (p<0.05) maiores do que os mesmos obtidos pelo processo convencional de porcelana fundida sobre o metal, para ligas de ouro e de CoCrMo. A prensagem a quente também introduziu uma melhoria significativa (p<0.05) na resistência ao corte da porcelana, relativamente ao processo convencional de cozimento da porcelana em vácuo. A quase completa ausência de defeitos, como poros, na interface metal-cerâmico e na própria porcelana estiveram na base das melhorias da ligação metal-cerâmico e da coesão de porcelana, respetivamente. A adesão entre o metal e o cerâmico foi também avaliada para diferentes tratamentos superficiais da subestrutura metálica, nomeadamente em superfícies polidas e superfícies rugosas. A porcelana apresentou maior adesão ás superfícies rugosas do que às superfícies polidas, dado que as superfícies rugosas permitiram uma maior retenção mecânica e também uma maior área superficial para promoção das ligações químicas. Neste trabalho foi feita a avaliação de uma liga de CoCrMo, obtida por fundição e por prensagem a quente, em termos da sua microestrutura, resistência à corrosão, dureza a resistência da ligação metal-cerâmico. A liga fundida apresentou uma microestrutra dendríticas enquanto a liga prensada a quente apresentou uma microestrutura globular. A maior dureza exibida pela liga prensa a quente está associada a uma microestrutura mais fina. Também as melhores propriedades de corrosão apresentadas pela liga prensada a quente, em relação à liga fundida, estão relacionadas com o seu tipo de microestrutura. Não foram encontradas diferenças significativas nos valores da resistência mecânica da ligação metal-cerâmico quando se usou a liga prensada a quente ou a liga fundida. O tratamento de pré-oxidação afetou significamente (p<0.05) a resitência da ligação metal-cerâmico, num estudo em que se usou uma liga dentária de CoCrMoSi. Os provetes não pré-oxidados apresentaram maiores valores de ligação metal-cerâmico que os provetes pré-oxidados/lixados. A presença de resíduos da camada de óxido na superfície do metal, após a sua remoção com lixa, bem como a formação de uma camada de óxido espessa na interface metal-cerâmico aquando do cozimento da porcelana, foram os fatores que estiveram na base da perda de resistênia da ligação dos provetes pré-oxidados. Todos os proveres pré-oxidados apresentaram falhas adesivas e mistas. O tratamento de pré-oxidação revelou um efeito prejudicial na adesão entre a liga de CoCrMoSi e a porcelana dentária. Vários compósitos metal/cerâmico foram testados como intercamadas com o objetivo de melhorar a resitência da ligação entre o metal e o cerâmico, seguindo uma abordagem dos materiais com gradiente funcional propriedades. Foram testados dois tipos de ligas metálicas, uma liga de alto teor de ouro e uma liga de CoCrMo. Ambas as ligas mostraram melhorias significativas (p<0.05) na resistência da ligação metal-cerâmico com o uso de uma transição gradual entre o metal e o cerâmico, por meio de uma intercamada de compósito metal/cerâmico. As partículas metálicas da intercamada atuaram como uma fase de reforço da matriz cerâmica, aumentando a resistência à tratura do compósito da intercamada e aumentando a resistência do sistemas metal-intercamada-cerâmico. A melhoria da resistência da ligação conseguida com o uso de uma intercamada, relativamente à ligação metal-cerâmico convencional, ascendeu a 140%. Os novos restauros dentários desenvolvidos com base no conceito de materiais com gradiente funcional de propriedades foram avaliados em termos do seu desempenho em condições de fadiga termo-mecânica, simulando as condições clínicas. A resistência da ligação destes novos restauros após fadiga térmica e mecânica foi significativamente (p<0.05) maior que a verificada para os restauros convencionais. A transição gradual de propriedades entre o metal e o cerâmico por via da introdução da intercamada de compósito na interface metal-cerâmico foi responsável pela melhoria do desempenho dos novos restauros dentários nos testes de fadiga. Com este novo sistema foram observadas melhorias na resitência da ligação metal-cerâmico, após fadiga, da ordem dos 210%. No final do trabalho foi feito um teste preliminar de execução de um restauro dentário metalocerâmico em coroas reais, aplicando o conceito de intercamada de compósito na interface entre o metal e o cerâmico. O processo foi executado com recurso à tecnologia atual de prensagem da cerâmica a quente e resultou numa boa qualidade da ligação metal-cerâmico. Não se verificou nenhuma restrição geométrica ou outras ao procedimento de restauro.
format Tese
author Henriques, Bruno Alexandre Pacheco de Castro.
Silva, Filipe Samuel Correia Pereira.
Soares, Delfim Fernandes.
Universidade do Minho.
author_facet Henriques, Bruno Alexandre Pacheco de Castro.
Silva, Filipe Samuel Correia Pereira.
Soares, Delfim Fernandes.
Universidade do Minho.
author_sort Henriques, Bruno Alexandre Pacheco de Castro.
title Bond strength enhancement of metal-ceramic dental restorations by FGM design /
title_short Bond strength enhancement of metal-ceramic dental restorations by FGM design /
title_full Bond strength enhancement of metal-ceramic dental restorations by FGM design /
title_fullStr Bond strength enhancement of metal-ceramic dental restorations by FGM design /
title_full_unstemmed Bond strength enhancement of metal-ceramic dental restorations by FGM design /
title_sort bond strength enhancement of metal-ceramic dental restorations by fgm design /
publishDate 2022
url https://app.bczm.ufrn.br/home/#/item/215006
work_keys_str_mv AT henriquesbrunoalexandrepachecodecastro bondstrengthenhancementofmetalceramicdentalrestorationsbyfgmdesign
AT silvafilipesamuelcorreiapereira bondstrengthenhancementofmetalceramicdentalrestorationsbyfgmdesign
AT soaresdelfimfernandes bondstrengthenhancementofmetalceramicdentalrestorationsbyfgmdesign
AT universidadedominho bondstrengthenhancementofmetalceramicdentalrestorationsbyfgmdesign
_version_ 1766842820865294336
spelling oai:localhost:123456789-1423802022-12-01T05:15:43Z Bond strength enhancement of metal-ceramic dental restorations by FGM design / Henriques, Bruno Alexandre Pacheco de Castro. Silva, Filipe Samuel Correia Pereira. Soares, Delfim Fernandes. Universidade do Minho. Engenharia mecânica - Tese. Restaurações metalocerâmicas - Dentes - Tese. Gradiente funcional de propriedades(FGMs) - Tese. Durabilidade - Sucesso - Tese. Abstract: Bond strength enhancement of metal-ceramic dental restorations by FGM design Metal ceramic dental restorations are widely used in dental prosthetics due to their good esthetic properties but mainly because of their higher survival rates when compared to other restorative systems. Nevertheless, they still encompass some medium to long term clinical failures, which puts patients back to the dentists' chair, causing uncomfortable interventions and undesired money expenditures. This work is concerned with the development of FGM's (Functionally Graded Material) based solution that enhances metal-ceramic bond strength aiming at increasing of long term survival rates of metal-ceramic dental restorations and with the study of the variables that affect metal-ceramic bond strength. The variables that were subjected to study were the hot pressing, the surface treatment, the type of processing used to produce metal substructures, and the preoxidation heat treatment. The hot pressing technique revealed to have significant (p<0.05) influence on the metal-ceramic bond strength, resulting in composites with significantly (p<0.05) higher bond strength values when compared to those obtained by conventional PorcelainFused-to-Metal technique for high gold dental alloys and for CoCrMo dental alloys. In the same way, the hot pressing technique also produced a significant enhancement on porcelain shear strength relative to the conventional vacuum sintered porcelain. The flawless metal-ceramic interfaces and the absence of pores within ceramics thus produced were regarded for the bond strength and cohesion improvements, respectively. The metal-ceramic adhesion was also assessed for different surface treatments of the metal substructure, namely polished and rough surfaces. Porcelain exhibited higher adhesion to rough metal substrates than to polished ones. The mechanical interlocking and the higher surface area for chemical bonding caused the bond strength improvements seen in rough surfaces. The CoCrMo alloy obtained by casting and hot pressing was assessed in terms of microstructure, corrosion resistance, hardness and metal-ceramic bond strength The casted alloy exhibited a dendritic microstructure whereas the hot pressed alloy exhibited a globular microstructure. The hot pressed alloy revealed higher hardness due to a finer microstructure. The finer microstructure was also regarded for the enhanced corrosion resistance of hot pressed alloys over casted alloy. No significant differences were found in metal-ceramic bond strength between the two types of processing techniques. The preoxidation heat treatment, performed in CoCrMoSi dental alloy, significantly (p<0.05) affected the metal-ceramic bond strength. Non-preoxidized specimens exhibited higher metal-ceramic bond strength than preoxidized/ground ones. The lower bond strength results observed in preoxidized/ground specimens were originated by the presence of oxide remnants on their metal surface after grinding and by the higher oxide thickness formed at the metal-ceramic interface. All preoxidized specimens exhibited adhesive failure type while non-preoxidized presented both adhesive and mixed failure types. Preoxidation heat treatment revealed a detrimental effect on the adhesion of CoCrMoSi-porcelain composites for dental restorations. Several metal/ceramic composites were used as interlayers aiming at the improvement of the bond strength between metal and ceramic, following a FGM approach. Two types of alloys were tested, namely a high-noble alloy and a CoCrMo alloy. Both alloys showed significant (p<0.05) improvements in the metal-ceramic bond strength when using a graded transition provided by the metal/ceramic composite interlayer. The metal particles of the composite interlayer acted as a reinforcing phase that increased the fracture strength of the composite interlayer and improved the strength of the metal-interlayer-ceramic system. The bond strength improvements, relative to conventional PFM technique, proved to be in excess of 140%. The newly developed FGM approach for dental metal-ceramic dental restorations was also evaluated in terms of its performance under thermo-mechanical fatigue conditions. These new functionally graded restorations showed significantly (p<0.05) higher performance under fatigue conditions relative to conventional PFM restorations. The bond strength results showed that the presence of a composite interlayer at the interface significantly (p<0.05) improves the adhesion between the two materials under fatigue conditions, relative to those found in conventional PFM technique. The reduction of the properties mismatch at the metal-ceramic interface of the functionally graded restorations was considered to be the main cause for the bond strength improvements after fatigue tests. Improvements in the range of 210% were observed for the most severe testing conditions. In the end of this work, a preliminary test comprising the manufacture of a graded metal-ceramic dental restorations in real crows were conducted. The restorations were fabricated using the hot pressing technology currently available in dental prosthetic laboratories. This process produced crowns with a good quality of the bond between metal and ceramic. Moreover, no geometric restraints or others were observed to the restorations' proceedings.#$&Resumo: Os restauros dentários metalocerâmicos são muito usados em prótese dentária devido às suas boas propriedades estéticas, mas sobretudo devido às suas elevadas taxas de sucesso clínico comparativamente com outros sistemas de restauro. Contudo, apesar de menos frequentes, também eles apresentam falhas clínicas a médio e longo prazo que fazem com que o paciente regresse à cadeira do dentista, causando intervenções desconfortáveis e gastos desnecessários de dinheiro. Assim, esta tese prende-se com o desenvolvimento de novos sistemas metal-cerâmico para restauro dentário recorrendo ao conceito dos materiais com gradiente funcional de propriedades(FGMs) tendo em vista o aumento da durabilidade e da taxa de sucesso clínico deste tipo de restauro. Esta tese também se debruçou sobre o estudo de variáveis que afetam o resitência da ligação metal-cerâmico. As variáveis alvo de estudo foram: a prensagem a quente, o tratamento superficial, o topo de processamento das substruturas metálicas e o tratamento de pré-oxidação. A técnica de prensagem a quente revelou uma influência significativa(p<0.05) na resitência mecânica da ligação metal-cerâmico, dando origem a compósitos com resitâncias de ligação significativamente (p<0.05) maiores do que os mesmos obtidos pelo processo convencional de porcelana fundida sobre o metal, para ligas de ouro e de CoCrMo. A prensagem a quente também introduziu uma melhoria significativa (p<0.05) na resistência ao corte da porcelana, relativamente ao processo convencional de cozimento da porcelana em vácuo. A quase completa ausência de defeitos, como poros, na interface metal-cerâmico e na própria porcelana estiveram na base das melhorias da ligação metal-cerâmico e da coesão de porcelana, respetivamente. A adesão entre o metal e o cerâmico foi também avaliada para diferentes tratamentos superficiais da subestrutura metálica, nomeadamente em superfícies polidas e superfícies rugosas. A porcelana apresentou maior adesão ás superfícies rugosas do que às superfícies polidas, dado que as superfícies rugosas permitiram uma maior retenção mecânica e também uma maior área superficial para promoção das ligações químicas. Neste trabalho foi feita a avaliação de uma liga de CoCrMo, obtida por fundição e por prensagem a quente, em termos da sua microestrutura, resistência à corrosão, dureza a resistência da ligação metal-cerâmico. A liga fundida apresentou uma microestrutra dendríticas enquanto a liga prensada a quente apresentou uma microestrutura globular. A maior dureza exibida pela liga prensa a quente está associada a uma microestrutura mais fina. Também as melhores propriedades de corrosão apresentadas pela liga prensada a quente, em relação à liga fundida, estão relacionadas com o seu tipo de microestrutura. Não foram encontradas diferenças significativas nos valores da resistência mecânica da ligação metal-cerâmico quando se usou a liga prensada a quente ou a liga fundida. O tratamento de pré-oxidação afetou significamente (p<0.05) a resitência da ligação metal-cerâmico, num estudo em que se usou uma liga dentária de CoCrMoSi. Os provetes não pré-oxidados apresentaram maiores valores de ligação metal-cerâmico que os provetes pré-oxidados/lixados. A presença de resíduos da camada de óxido na superfície do metal, após a sua remoção com lixa, bem como a formação de uma camada de óxido espessa na interface metal-cerâmico aquando do cozimento da porcelana, foram os fatores que estiveram na base da perda de resistênia da ligação dos provetes pré-oxidados. Todos os proveres pré-oxidados apresentaram falhas adesivas e mistas. O tratamento de pré-oxidação revelou um efeito prejudicial na adesão entre a liga de CoCrMoSi e a porcelana dentária. Vários compósitos metal/cerâmico foram testados como intercamadas com o objetivo de melhorar a resitência da ligação entre o metal e o cerâmico, seguindo uma abordagem dos materiais com gradiente funcional propriedades. Foram testados dois tipos de ligas metálicas, uma liga de alto teor de ouro e uma liga de CoCrMo. Ambas as ligas mostraram melhorias significativas (p<0.05) na resistência da ligação metal-cerâmico com o uso de uma transição gradual entre o metal e o cerâmico, por meio de uma intercamada de compósito metal/cerâmico. As partículas metálicas da intercamada atuaram como uma fase de reforço da matriz cerâmica, aumentando a resistência à tratura do compósito da intercamada e aumentando a resistência do sistemas metal-intercamada-cerâmico. A melhoria da resistência da ligação conseguida com o uso de uma intercamada, relativamente à ligação metal-cerâmico convencional, ascendeu a 140%. Os novos restauros dentários desenvolvidos com base no conceito de materiais com gradiente funcional de propriedades foram avaliados em termos do seu desempenho em condições de fadiga termo-mecânica, simulando as condições clínicas. A resistência da ligação destes novos restauros após fadiga térmica e mecânica foi significativamente (p<0.05) maior que a verificada para os restauros convencionais. A transição gradual de propriedades entre o metal e o cerâmico por via da introdução da intercamada de compósito na interface metal-cerâmico foi responsável pela melhoria do desempenho dos novos restauros dentários nos testes de fadiga. Com este novo sistema foram observadas melhorias na resitência da ligação metal-cerâmico, após fadiga, da ordem dos 210%. No final do trabalho foi feito um teste preliminar de execução de um restauro dentário metalocerâmico em coroas reais, aplicando o conceito de intercamada de compósito na interface entre o metal e o cerâmico. O processo foi executado com recurso à tecnologia atual de prensagem da cerâmica a quente e resultou numa boa qualidade da ligação metal-cerâmico. Não se verificou nenhuma restrição geométrica ou outras ao procedimento de restauro. 1 2022-10-06T11:33:12Z 2022-10-06T11:33:12Z 2012. Tese 621 H519b TESE 215006 https://app.bczm.ufrn.br/home/#/item/215006 https://app.bczm.ufrn.br/home/#/item/215006